Acetic acid corrosion

2019-01-24 View Original

Thread Content

At a medium temperature of 100 degrees Celsius, with 99% water and 1% acetic acid and hydrocyanic acid, will 316L metal suffer from corrosion?
Reply #2 2019-01-24
Mixed acid – I wonder too whether the client will conduct hanging slice tests at various concentrations
Reply #3 2019-01-24
The actual situation now is that corrosion is occurring, but it’s not clear whether it’s hydrocyanic acid that is causing corrosion of the stainless steel, or if there are other reasons behind it
Reply #4 2019-01-28
What device is it? What’s the pressure? If it is a heat exchanger, graphite heat exchangers are recommended.
Reply #5 2019-01-28
In comparison, hydrofluoric acid is the main factor causing corrosion of 316L. Under such operating conditions, non-metallic materials can be considered as the material for heat exchangers.
Reply #6 2019-01-29
Are 316L also used for the inlet and outlet pipes of the pump? Is there any corrosion?

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.