Heating furnace drying

2021-06-09View Original

Thread Content

Why, during the heating process of the furnace, should the temperature of the medium at the outlet of the furnace tubes be no more than 350°C for carbon steel tubes, and no more than 450°C for chromium-molybdenum steel tubes? What is the basis?
Reply #22021-06-09
Refer to SH/T3115.
Reply #32021-06-17
Different furnace tube materials have different allowable temperature limits
Reply #42021-06-18
This is mainly because the materials of the two are different, as are their temperature resistance ratings. Chromomolybdenum steel has a higher temperature resistance rating than ordinary carbon steel.
Reply #52021-06-18
Please provide the full standard name as well as the relevant clauses of the standard; a screenshot would be ideal
Reply #62021-07-03
Thank you, sir. It’s in Appendix A, but it’s not the screenshot you sent; moreover, only the data for carbon steel at 350 degrees was found, and no data for chromium-molybdenum steel was found. . .

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.