The temperature of the transformed gas rises too quickly – low-washing treatment?

2014-12-31 View Original

Thread Content

May I ask a question? The main material is 16MnR; it is a fixed-tube-sheet heat exchanger. When the temperature on the tube side changes rapidly, what should be the maximum allowable rate of change? I believe it should be 5 degrees Celsius per minute
Reply #2 2014-12-31
This post was last edited by sxtblo on 2014-12-31 at 17:20. When the temperature is high and the amount of saturated moisture increases, it is necessary to increase the amount of methanol used for spraying; if a cooler is available, then increase the amount of cooling water or refrigerant used

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.