Problems with pipeline welding

2022-06-23View Original

Thread Content

It is being carried out on-site, and as a process engineer, I’m not sure whether this approach is appropriate. I would appreciate guidance from the experienced experts in this forum. The original pipe wall thickness was 10, while the wall thickness of the tee purchased now is 12.7. Can they be welded together? Combustible gas pipeline, pressure 3.2 MPa, temperature 220°C. The construction party said that welding can be done after grinding the groove. Are there any standards or requirements? I hope the experienced members of this forum can give me some guidance!
Reply #22022-06-23
This post was last edited by lijie2007521 on 2022-6-24 at 16:13. Welding is possible; there’s no issue with that. The welding groove specifications can be found in GB/T985.1. If you’re not sure, you can contact me, Chuanyou.
Reply #32022-06-24
Sure. If the two thicknesses are different, edge trimming can be carried out in accordance with GB150.4-P325

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.