FCC pre-rising section temperature

2017-04-11View Original

Thread Content

What are the minimum and maximum temperatures for the coaxial pre-lift section? What are the disadvantages of being too low or too high? I hope to receive guidance from all the teachers!
Reply #22017-04-12
As long as the reaction temperature is met, a lower temperature in the pre-raising section and a higher oil-to-agent ratio are acceptable; however, if the temperature is too low, it will affect the vaporization and cracking reactions upon contact with the feedstock, potentially leading to coking in the riser or the settler.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.