Amount of passivator injected

2019-02-03View Original

Thread Content

What are the main criteria used to determine the amount of passivator to be injected into a catalytic cracking unit?
Reply #22019-02-15
Analysis data of the re-injected fluid: the antimony-nickel ratio; the methane/hydrogen ratio in the dry gas prior to removal is no greater than 2
Reply #32019-02-16
It should be that the hydrogen/methane ratio in dry gas is no more than 2. But why is there a requirement that this ratio must not exceed 2?

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.