Excessive cold-high-purity ferric ions

2012-06-14View Original

Thread Content

We have a 200,000-ton catalytic hydrogenation reforming unit here, and recently the level of ferric ions has often been above the acceptable limit, while the pH value is normal. Could experts tell me what might be causing this?
Reply #22012-06-20
This post was last edited by yuchenchf on 2012-6-20 at 15:32. It might be caused by the acid in the reactor dissolving iron; we can discuss this!
Reply #32012-06-21
I agree with the view above: the impurities in catalytic diesel generate acidic substances during the hydrogenation process, which can cause corrosion to the equipment through which it flows; as a result, the iron ion level becomes excessive. There is very little acidic corrosive medium, and the pH value shows no significant change.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.