On the corrosion margin of pipelines

2012-08-17View Original

Thread Content

What should be the corrosion margin for Q345R pipes with a cast layer?
Reply #22012-08-17
The corrosion allowance of pipelines depends not only on the material but also on the medium inside the pipeline and the design life (usually 15 years). For carbon steel, a value of 1.6 mm is generally used when corrosion is not severe; 3.2 mm is used when corrosion is more severe. In special situations such as erosion by solid particles, a value greater than 3.2 mm should be chosen depending on the specific conditions.
Reply #32012-08-17
Okay, thank you! Are there any standard regulations for this? For example, like the regulations for containers specified in HG/T 20581-2005...
Reply #42020-10-25
The pipeline design codes also specify corrosion margins under various conditions

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.