Regarding the heat treatment time after cladding of the tube sheet

2012-10-12View Original

Thread Content

Dear everyone, how is the holding time for stress-relief heat treatment after tube sheet surfacing determined? Some design documents specify it as the tube sheet thickness plus the surfacing layer thickness. I think the butt welds can be considered in this way, but for surfacing welding, isn’t it taking too long to consider the thickness of the tube sheet? I would appreciate it if those who are aware could offer some advice
Reply #22012-10-12
Link: http://bbs.hcbbs.com/thread-671458-1-1.html. I agree with the view in post 2.
Reply #32012-10-12
I think it has to do with the material of the base metal and the material used for surfacing; everything else is secondary
Reply #42012-10-12
The heat treatment mentioned here is the stress-relief treatment after cladding of the tube sheet, and it is not a heat treatment intended for other purposes.
Reply #52012-10-12
That’s not the same either; can chrome-molybdenum steel and Q345 be the same?

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.