Why, at the same high temperature, does 310H not have a higher allowable stress than 304H?

2007-12-25View Original

Thread Content

Question: Why, at the same high temperature, does 310H not have a higher allowable stress than 304H? Can 304H be used at higher temperatures than 310H? Superheated steam, 800℃
Reply #22008-01-26
Isn’t there anyone who deals with materials here?
Reply #32008-01-26
I want to know too, you experts in materials

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.