Welding process of 14mm16MnR product welding test plate

2008-01-21View Original

Thread Content

Let’s talk about the welding process parameters of your company’s 14mm thick 16MnR product welding test plate - the value that can be achieved after several times of welding with wire and flux - 20 degrees impact
Reply #22008-01-21
The 14mm thick plate must be welded by front and back automatic welding. After beveling, it will be unqualified at -20 degrees. If the influence of welding process parameters is not considered, flux used at -40 degree level can be used. Welding wire: H10Mn2; flux: SJ101 3 times ; current: 550-650A voltage: 32-36V

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.