Regarding the equipment material issues of ammonium bisulfate aqueous solution

2008-01-26View Original

Thread Content

  There should be no problem in choosing 316 or 316L for equipment or pipe materials with 10 to 15% ammonium bisulfate aqueous solution. But what will happen if I choose 304 or 321? Is it applicable? Please talk to someone with experience!
Reply #22008-12-17
How about using corten steel?
Reply #32008-12-19
Under normal temperature conditions, if there is no miscellaneous acid, either 304 or 321 will work.
Reply #42013-09-09
If the concentration is 80%, what should we choose?

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.