How to weld 20 tubes together with Cr5Mo elbows without affecting strength
Reply #22008-02-21
For thicknesses of 8mm and below, the welding materials H10MnSi+J427 can be used; preheating at 250°C is required, followed by heat treatment at 680±10℃ for 0.5 hours. The evaluation standards are JB4708. This post was last edited by ssmith2007 on 2008-2-21 at 20:59
Reply #32008-02-21
Take a look at this to see if it helps: http://bbs.hcbbs.com/viewthread.php?tid=154774&extra=page%3D1&frombbs=1
Reply #42008-02-22
When welding 20 tubes to Cr5Mo elbows, it is necessary to first use TIG welding for the root pass, followed by MIG welding; a weld rod of a higher grade should be used, such as I307, so that the welding does not affect the strength of the steel.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.