The percentage of radiographic inspection of welded joints in the SH 3501 standard is an aspect related to the acceptance level

2008-02-25View Original

Thread Content

SHD grade in SH 3501 standard, t
Reply #22008-02-26
Does no one on this forum know the answer to this question?
Reply #32008-06-29
Because in low-temperature environments, the impact toughness of materials decreases sharply. When there are relatively severe defects, it can lead to a decrease in the stress capacity of the weld, causing cracks to occur under lower stresses, and as a result, the release of flammable and toxic substances within the pipeline

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.