Please tell me about the welding of chromium-molybdenum alloy steel and stainless steel

2008-02-28View Original

Thread Content

What is the welding process of chromium-molybdenum alloy steel and stainless steel? For example, 304 and 12CrMo, do they need preheating before welding and heat treatment after welding? Thank you
Reply #22008-02-29
Please refer to sh/T3520-2004 "Petrochemical Industry Chromium-Molybdenum Heat-Resistant Steel Welding Regulations":)
Reply #32008-02-29
When design conditions do not require it, preheating and heat treatment are not required for 304 and 12CrMo using A307 or nickel-based electrodes. Welding process qualification needs to be done before welding.
Reply #42008-02-29
Preheating before welding and stress elimination heat treatment after welding should be carried out! Welding materials should use 182 welding rod!
Reply #52008-03-02
The welding material is Ni182 electrode, which is NiCrFe-3

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.