After welding Hastelloy, the weld seam can only be ground with a grinding wheel – why cannot it be pickled? ?

2009-01-21View Original

Thread Content

After welding Hastelloy, the weld seam can only be ground with a grinding wheel – why cannot it be pickled? ?
Reply #22009-11-09
Is the poster the manufacturer that processes and produces Hastelloy? Under inquiry. . . Please contact me; I want to create a C-2000 device. Acid washing is not an option, probably because there is concern that elements such as Cl- in the acid wash solution could damage its corrosion resistance. I’m not sure about this, so I hope someone with more knowledge can clarify it for me. Thank you
Reply #32009-11-09
Since Hastelloy B-2 is sensitive to oxidizing media, a large amount of nitrogen-containing gases are generated during the pickling process, making it unsuitable for use. The above Baidu results~
Reply #42015-03-27
I don’t know either, I learned it*:):):):):):):):)
Reply #52015-03-27
Special grinding wheels must also be used, and the working environment needs to be clean. . . . Otherwise, there would be nothing to play;P

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.