When the operating temperature of SA516 GR70 is 427℃, what should be considered in the design?

2009-02-05View Original

Thread Content

Whether it is necessary to limit the carbon content, whether to use normalizing plates, whether to require heat treatment, whether to preheat before welding, etc. Ask everyone for advice!
Reply #22009-02-08
The temperature is so high, can you consider using other materials? High temperature resistant, such as CrMo steel? At least I think it is necessary to conduct high-temperature tensile tests on the materials to verify the mechanical properties at the design temperature.
Reply #32009-02-08
I agree with the suggestion above, it is best to change the material. The material used by the poster is ASME material which is equivalent to 16MnR. You should also pay attention to the tendency of graphitization.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.