How to address saltwater penetration in stainless steel pipe welds

2009-02-11View Original

Thread Content

Saline solution (containing NACL and a small amount of NA2CO3) keeps seeping out from the welds of the stainless steel pipes; the temperature of this saline solution is around 80–90 degrees. Thank you
Reply #22009-02-12
Post-welding solid solution treatment. Last edited by bingyu252 on 2009-2-12 08:47.]
Reply #32009-02-12
First, verify whether there are any issues with the stainless steel material being used, as saltwater is highly corrosive at this temperature. Additionally, the welding process must be strictly followed. Since leakage has occurred, if it is not due to corrosion-induced perforations, then there are cracks present. The formation of welding cracks is mentioned in various stainless steel welding procedure manuals, which can be referred to for further information.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.