Reduction method for nickel-based hydrogenation catalysts?

2009-03-08View Original

Thread Content

Reduction method for nickel-based hydrogenation catalysts? I seek advice from all the experts here! Thank you. This post was last edited by zxh6267 on 2009-3-9 08:05.]
Reply #22009-03-09
Nickel-based hydrogenation catalysts are typically reduced using hydrogen, and the temperature can be slowly raised to 480 °C under normal or pressurized conditions, with this temperature being maintained for 6 hours.
Reply #32009-03-10
Nickel can be used as a catalyst and hydrazine hydrate as a reducing agent
Reply #42012-03-30
I earnestly request information on the reduction step using nickel-containing catalysts as well as relevant precautions; I hope experts can offer their guidance! !
Reply #52012-04-01
It’s a highly mature technology, with two processes: continuous and batch. In the batch process, a small amount of catalyst is added in several batches, while in the continuous process, the catalyst is added continuously.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.