Regarding the issue of chrome plating allowance

2009-03-09View Original

Thread Content

Please discuss the issue of leaving a margin for chrome plating. For example, a sleeve is 40 in length, and the outer circle and inner hole drawings require dimensions of Φ35-0.01 and Φ10+0.01 respectively. The technical requirements are chrome plating D·YCr10 and heat treatment to reach a hardness of HRC58-62. What should its process flow be like? This post was last edited by flower716- on 2009-3-9 09:54 ]
Reply #22009-03-09
I think it should be like this: Carry out heat treatment after leaving a margin, then grind the outer circle and inner hole to Φ35-0.01 -0.02, Φ10 +0.02 +0.01, then D·YCr20, and finally grind to the drawing size Φ35-0.01, Φ10+0.01.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.