Is heat treatment required for spot welding on a 1Cr9Moφ127×10 pipeline?

2009-03-29View Original

Thread Content

Is heat treatment required for spot welding on a φ127×10 pipeline made of 1Cr9Mo?
Reply #22009-03-29
Spot welding usually does not require heat treatment
Reply #32009-03-29
If heat-resistant steel electrode R507 is used, preheating to 200 degrees is required before welding, followed by heat treatment that must be completed within 24 hours after welding. Additionally, per the requirements for heat treatment, the same weld area cannot undergo more than 2 rounds of heat treatment. Using austenitic welding rod A307 is quite simple; spot welding is sufficient, and there are no special requirements. I recommend using this method!
Reply #42009-03-29
Although it is a high-pressure pipe, heat treatment may not be required.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.