Why can’t the synthesis tower overheat when ammonia pressure is increased? What are the harms?

2009-04-05View Original

Thread Content

Full-circulation aqueous solution method: Why can’t the synthesis tower overheat when ammonia pressure is increased? (
Reply #22009-04-06
Excessive temperature has an impact on the lining and welds of the synthesis tower
Reply #32009-04-06
This type of over-temperature results in a sudden rise in the temperature inside the tower; a large difference arises between the temperature inside the tower and the temperature of the tower walls, which can easily damage the lining.
Reply #42009-04-08
In a synthesis tower, the ammonia pressure should generally not exceed 150 degrees before feeding can begin; excessive temperature during this pressure increase can lead to uneven deformation between the tower lining and the tower walls, causing significant damage.
Reply #52009-04-27
Is overheating always a sudden rise in local temperature? It is only sudden increases that cause a sharp rise in stress, right?

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.