2009-04-08View Original

Thread Content

Everyone, please help and tell me what the heat treatment temperature should be for Q345R+00Cr17Ni14Mo2 (14+3) materials after the equipment has been manufactured
Reply #22009-04-08
Since this thickness is relatively thin and it is welded to stainless steel, post-weld heat treatment is generally not required.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.