On page 128 of the specification, under H2S stress corrosion, the material usage state is required to be at least normalizing + tempering, annealing, and quenching and tempering. Excuse me, should I choose one of the three usage statuses, or should I do all three?
Reply #22009-04-15
Of course, it is a matter of choosing one out of three. A material cannot be in three states at the same time.
Reply #32009-04-15
The HG standards are more detailed.: The material usage state should be at least normalizing or normalizing + tempering, annealing, and quenching and tempering. That should mean that it’s enough to at least achieve one of the above.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.