What is the standard temperature of the weld after welding that is required before conducting a hydrostatic test? (Urgent)

2009-08-21View Original

Thread Content

What temperature standard must the weld reach after welding before a hydrostatic test can be conducted? Are there specific standard regulations? Could some expert please give me some guidance?
Reply #22009-08-21
This question is a bit unclear; the temperature of the weld after welding needs to be reduced to room temperature before testing can be carried out. And it’s impossible to weld the entire pipeline at once and finish welding it all in one go
Reply #32009-08-22
2# Kuanhai is not a pipeline as a whole, but rather an individual valve. After a set of valves is welded together, a hydrostatic test must be carried out. I’m not sure where such standards can be found; I’d like to learn more about this

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.