Material issues with the oil cooler of vinyl chloride screw compressors

2009-10-16View Original

Thread Content

Our factory uses Fuda’s LU450W7T screw compressors, with oil cooling achieved through water cooling. I would like to know what material is suitable for the cooler – copper or stainless steel? If copper is chosen, will it have any impact on the equipment’s service life?
Reply #22009-10-19
Copper should not be used, as the crude product contains acetylene, which can cause an explosion. I think it’s made of stainless steel.
Reply #32009-11-13
In principle, the presence of copper is not allowed; it may also be necessary to consider the copper content, and stainless steel is recommended.
Reply #42011-04-21
Coolers for Fuda vinyl chloride compressors are available; feel free to contact us at QQ535628705.
Reply #52011-04-21
Our factory also uses a Futakawa model, specifically the LU450W-7T, which is water-cooled as well. I don’t think the material of the cooler is copper.
Reply #62011-04-21
Stainless steel is better; copper reacts with acetylene

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.