One tank, with a diameter of 2400; the main material is Q235B. It is required to apply a layer of anti-corrosion coating on the inner surface. I was wondering whether it’s possible to conduct a hydrostatic test after applying the paint Another thing is how to make painting easier. If both end caps are welded in, the space inside is limited, making it difficult to remove rust; moreover, painting releases a strong odor ; I was wondering if anyone has any better suggestions?
Reply #22009-10-18
It’s possible to carry out processing first and then welding, but the part still needs to be processed again after welding; safety must be taken very seriously.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.