This post was last edited by ssdh on 2009-10-20 08:39. The wall of the hollow fiber membrane spun is too thin. What should I do?; I once increased the spinning fluid flow rate, but it felt like the core fluid flow was not enough. Is this situation related to the spinneret?
Reply #22009-11-08
Generally suitable for spinnerets, which are directly related to each other. Different spinnerets have different specifications.
Reply #32009-11-08
It's mainly a problem with the specifications of the spinneret, or maybe it's a problem with the formula of the casting fluid? Try changing the ingredient ratio in the recipe.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.