Our factory produces potassium fluosilicate through a double-displacement reaction using fluosilicic acid and potassium chloride; the semi-finished product is then dried after filtration. However, the quality of the product does not reach 98% at all. I would be grateful if any experts with relevant expertise could offer guidance, and technical cooperation would also be acceptable if possible. My email address is henly001@163.com. I have asked similar questions in other forums, but no one answered them; I hope the experts and veterans in this forum can offer some guidance.
Reply #22009-11-19
May I ask what the main impurities are? Has any analysis been done?

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.