Technical assistance: Anion resin exchange

2010-01-04View Original

Thread Content

This post was last edited by hesonchang214 on 2010-1-31 08:33. Our company wants to reuse steam condensate as process water, but the chloride concentration in it is 5.5 mg/l. We’re not sure what methods can be used to treat it; if anion exchange resins are used, is it necessary to perform backwashing and forward washing?
Reply #22010-01-04
When the chloride ions reach a certain level, it is of course necessary to regenerate the resin. Otherwise, the function of the resin will be affected.
Reply #32010-01-04
It’s not what the person upstairs meant; I want to use an anionic resin to remove chloride ions from the condensed water.
Reply #42010-01-05
3# heiying004 No matter what you plan to do, if you use resin, it will lose its effectiveness after operating for a while; therefore, it is necessary to carry out backwashing and regeneration in order to restore its ion exchange function.
Reply #52010-01-17
It is recommended to use a weak resin for treatment; normal processing procedures can be followed.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.