Corrosion allowance for metal pipes in petroleum refining and chemical enterprises

2010-02-07View Original

Thread Content

Can pipelines in refining and petrochemical enterprises that have reached or are close to the corrosion allowance still be used?
Reply #22010-02-07
Yes! But strength verification is required! First, calculate the design wall thickness using the film stress theory; the design wall thickness plus corrosion allowance plus rounding plus negative deviation equals the nominal wall thickness. In fact, due to the very small inner diameter of the pipes, their wall thickness is quite thin. Since standard pipes are selected based on their nominal wall thickness, the roundness values are usually quite high. Although there is no corrosion margin left, these roundness values are still more than sufficient to ensure the required strength

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.