How should bent or deformed furnace columns be dealt with?

2010-02-26View Original

Thread Content

Urgently need a plan to adjust the furnace column! ! ! Dear sea friends, please give some advice
Reply #22010-02-26
You should make it clear to what extent the transformation takes place How many transformations? What is the cause? Replacing the furnace column is a last resort.
Reply #32010-02-27
The situation needs to be detailed before a repair or replacement plan can be formulated based on the actual conditions
Reply #42010-02-27
It is necessary to clarify the deformed area of the furnace column and the curvature of that specific furnace column.
Reply #52010-02-27
Please provide an explanation of the reasons for the deformation and the extent of it, so that we can analyze it together.
Reply #62010-02-28
The reason for this situation is that the pressure and temperature control systems in the coke oven are not properly managed; both replacement and maintenance only provide temporary solutions, and it is necessary to identify the root causes.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.