What are the causes of ceramic cracks or spalling in ceramic lined pipes?

2010-03-11View Original

Thread Content

I would appreciate the help of experts: In our plant, there are 4–5 cracks in the ceramic linings of the tees and elbows; moreover, the ceramic material has peeled off at the pipe ends. The gases flowing through these pipes are HCL gas and silicon powder, and the temperature is around 200 degrees. What could be the cause of this? Thank you.
Reply #22010-03-11
Has there been any change in temperature? At such high temperatures, if the temperature fluctuates, cracks will appear in the ceramics! There might be other reasons as well; experts, please keep answering!
Reply #32010-03-11
It’s probably due to the temperature difference; high air pressure could also be a factor

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.