2010-04-01View Original

Thread Content

What to do if too much thiourea is added to the copper melt?~? ? ~? ~Is there any way to remove it~? ? ~? ~? What are the decomposition temperatures of thiourea and soy gum? ~? ~? ~Please, everyone, help me out! ! ! ! ~~! !
Reply #22010-04-01
Thiourea, also known as thiourea, has a molecular weight of 76.12 and a melting point of 180–182°C; it decomposes at higher temperatures. Sublimes at 150~160°C under vacuum. Soluble in water, readily soluble in hot water; dissolves in ethanol when heated, almost insoluble in ether. It hygroscopically absorbs moisture from the air and is flammable. It has low toxicity but is corrosive to the skin. The decomposition temperature of bean gum is probably around 310 degrees. The dissolution temperature of bone glue is between 65 and 75 degrees; above 100 degrees, molecular decomposition begins, leading to aging of the substance. A slightly higher amount of thiourea should be fine; the original poster didn’t specify a exact quantity. If I add too much, I can only draw out a portion of the electrolyte and replace it with fresh liquid in order to balance the amount of thiourea in the system.
Reply #32010-04-03
Thiourea and soy gum are organic solvents; if they need to be removed, they can be oxidized using hydrogen peroxide, which allows for their removal without introducing any other impurities.
Reply #42010-04-06
Hydrogen peroxide? ? ? How much should be added? 3# Mountain Breeze
Reply #52010-04-06
What is the reason why the copper plates become brittle and cannot be peeled off? ~? ? ~? ~?
Reply #62010-04-08
Thiourea and gelatin are used together. For dissolution, our company uses high-pressure steam; thereafter, the mixture is added to a storage tank in an even manner. If there is an excess amount, additional water is added to dilute it, or the amount used in the second cycle can be reduced accordingly. The chlorine content should also be increased appropriately. What is the reason behind the copper plates becoming brittle and unable to be peeled off? ~? There are many influencing factors. Without specific details, it’s impossible to conduct an analysis.
Reply #72010-04-08
The copper plate is brittle. Moreover, one side of it is smooth while the other side has particles on it; even the smooth side is quite brittle``
Reply #82013-11-17
How to determine the amount of additive in the cathode plate 12 hours after being placed in the tank
Reply #92013-11-26
The issues raised by the original poster are all core technologies held by various manufacturers; without hiring experts to address them specifically, trying to figure things out on one’s own will take a long time and incur significant costs (this is true only if one already has a cathode furnace), making it very difficult to find solutions to these problems!
Reply #102013-12-27
It usually relies on experience. First, check the color; second, listen to the sound when it is tapped

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.