2010-04-20View Original

Thread Content

Can F4-lined pipes be used in strong acid pipelines? Is there any temperature requirement for concentrated sulfuric acid above 90%?
Reply #22010-04-22
Pipes lined with F4 can be used for concentrated sulfuric acid, as well as high-temperature concentrated sulfuric acid. The main thing is to ensure the quality of Shenli.
Reply #32010-04-22
F4 materials can be used in strong acids and alkalis of any concentration at temperatures below 200 degrees without any problem.
Reply #42010-04-22
It can be used, but you have to check the quality
Reply #52010-04-22
For concentrated acid and dilute acid, negative pressure must be avoided.
Reply #62010-04-22
Why do strong acid pipelines in dry suction systems not use steel-lined PTFE pipes? What are the disadvantages?
Reply #72010-04-23
Steel-lined PTFE pipes are relatively expensive and have restrictions on use. They cannot be operated under negative pressure, otherwise the lining will fall off.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.