Selection of welding materials for composite steel plate Q245R+06Cr13Al?

2010-05-04View Original

Thread Content

As the title suggests, I would appreciate some guidance from those who are more experienced; I haven’t used 06Cr13Al very often in the past
Reply #22010-05-14
This post was last edited by Loulan Meng on 2010-5-14 at 16:08. Bevels are created on both sides of the steel plate, and the overlay layer is planed off to a width of 10 millimeters. For welding the base layer, automatic welding wire can be used; fluxes such as SJ101 or HJ431 are suitable, while for manual welding J427 is recommended. Preheat to 100 degrees for plate thicknesses greater than 30 millimeters. After the substrate is fully welded, RT and PT inspections are carried out; once it passes these inspections, cladding is applied. The transition layer is made of A302, while the cladding layer is made of A102.
Reply #32010-05-16
It seems wrong to say that A102 should be used, based on my personal opinion

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.