Issues with the valve internals?

2010-05-20View Original

Thread Content

What are the differences between hardening treatment and ST stainless steel cladding for valve internals, and which of these is more suitable for steam at around 200 degrees Celsius?
Reply #22010-05-20
For 200-degree steam, it seems that carbon steel material is sufficient
Reply #32010-05-21
I work in design, and from a basic perspective, I think that joints made by welding tend to come loose easily; hardening treatment is a better option. It’s hard to say whether the hardness achieved through hardening treatment will meet the required standards! Moreover, it becomes more brittle after hardening, which reduces its reliability!

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.