The boss said that selling tar resulted in too big a loss:$
This one? There are many ways to think of it. May I ask, what type of coke oven is it?
Reply to 2# enough067: 4.3m dual-bottom exhaust gas recirculation single-heater type ramming coke oven
When dehydrating, just remove less water, or lower the level of the liquid in the machine tank.
How are your procedures for tar dehydration established?
Dude, it’s the same as the one used in our factory. Hehe, the tar content is less than 2%; for external sales, 4% is the maximum allowed. The managers at Taiyuan Iron and Steel’s coking plant feel they’re losing out, as they keep pressing us to increase the amount used. But the results when exceeding that limit are really good. Well, what can we do?
Bro, you can control the moisture level by adjusting the height of the overflow weir plates and the amount of heating steam used in the tar tank – these are the most direct methods, and they should yield immediate results.
I have a way; I can also handle your wastewater for you. It’s a paid service, haha........
The simplest way is to increase the amount of tar sent out, so it can be sold more quickly
For example, on the 7th floor: The overflow weir issue of super centrifuges can be adjusted, and their efficiency in separating water is related to the height of the overflow weir. I increased it here because of the high water level; you can lower it a bit. The simplest way is to add ammonia directly to the storage tank, haha