Can 304 wire mesh packing be pickled with nitric acid?

2010-09-06View Original

Thread Content

Can 304 wire mesh packing be pickled with nitric acid?
Reply #22010-09-29
Yes, low-concentration nitric acid can be used, but care must be taken to rinse off any residual cleaning solution. It is rather difficult to clean the screen thoroughly.
Reply #32010-09-30
304 mesh packing can be pickled with nitric acid, but it is recommended to use dilute nitric acid with a concentration of less than 65%.
Reply #42010-10-01
If the concentration is low, it can be used~ Regular ceramic packing is commonly used in acidic solutions.
Reply #52010-12-03
Clean 304 mesh packing using nitric acid alone?
Reply #62010-12-03
Using a low concentration of nitric acid should be fine, as long as proper cleanup is carried out afterwards

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.