In the wall thickness calculation formula, is [σ]t the allowable stress of the steel plate or the allowable stress of the weld material?

2010-09-25View Original

Thread Content

This post was last edited by Lantian on 2017-6-2 at 14:11. As the title suggests, in the wall thickness calculation formula, does ‘t’ refer to the allowable stress of the steel plate or the allowable stress of the weld material? Thank you all
Reply #22010-09-25
It is the allowable stress of the steel plate at the design temperature
Reply #32010-09-25
It is the allowable stress of the steel plate; standards stipulate that the strength of the weld must not be lower than that of the base material.
Reply #42010-09-25
It’s of course the allowable stress of the steel plate; after multiplying it by the weld coefficient, we get the allowable stress for the weld area
Reply #52010-09-25
It should be the allowable stress of the steel plate at the design temperature

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.