How to improve the lifespan of the oxygen lance in lead smelting using bottom-blown furnaces?

2010-10-20View Original

Thread Content

The oxygen lance in lead bottom-blown furnaces is protected by nitrogen and cooling water; what measures can be taken to increase the lifespan of the oxygen lance? Please share your opinions, experts
Reply #22010-10-31
In my opinion, during the production process, stabilizing the materials and the oxygen-to-material ratio can help increase the usage time of the oxygen lance. If you want to achieve breakthrough progress, you need to consider the materials and design; it’s best to consult an industrial manufacturing engineer.
Reply #32010-11-09
At present, there is no oxygen lance material with better cost-performance. The proper control of the oxygen-to-nitrogen ratio and the amount of cooling water, along with the furnace temperature and the level of the lead slag, all have an impact on the lifespan of the oxygen lance.
Reply #42010-11-30
Is a straight shape more suitable or an axe-shaped one for the oxygen lance brick sleeves (7 pieces)? What are the specifications?

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.