Why do small chipping and bright spots appear at the arc edges after 6.5-inch silicon rods are cut into silicon wafers?
Reply #22011-08-10
Quality control for silicon wafer cutting includes: the tension of the steel wire, the moving speed of the steel wire, the feeding speed of the workpiece, and the cutting capability of the slurry.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.