Thermal potassium alkali method for decarburization

2011-01-20View Original

Thread Content

How to select the appropriate potassium carbonate concentration in thermal potassium-alkali decarburization?
Reply #22011-01-20
The concentration is roughly between 200 and 240
Reply #32011-01-21
A potassium carbonate concentration of 25–28% (by mass) is appropriate; if the concentration is too high, the solution will crystallize and get clogged, while if it is too low, the solution’s absorption capacity will be reduced.
Reply #42011-01-21
In the thermal potassium-alkali method for carbon removal, the alkali concentration refers to the total amount of potassium carbonate and potassium bicarbonate, known as the total alkali level; this value should be maintained between 27% and 30%. It is potassium carbonate that plays a key role in this process. If its concentration is too low, the CO2 absorption efficiency is poor, while if it is too high, the gas-liquid contact is inadequate. Moreover, alkali corrosion increases and blockages are more likely to occur

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.