The welded open-end fitting is tilted beyond the allowable limit; the issue of reshaping it using heat

2011-05-08View Original

Thread Content

For perforated connectors, fixtures are generally used for fixing them during welding; even so, it is easy for the horizontal alignment of the connector flanges to be out of spec after welding. On containers where requirements exist regarding the surface roughness, spot welding must be used instead of fixtures during welding, and the horizontal alignment still tends to be significantly off spec. In workshops, heating the components with fire is usually followed by using guide chains and hammers to adjust their alignment. . . . I would like to ask if GB ASME has any regulations or requirements regarding such matters
Reply #22011-05-11
Can stainless steel be grilled too? Does forced alignment not affect weld quality?
Reply #32011-05-11
I’m just worried it might cause problems, that’s why I’m seeking advice
Reply #42011-05-11
That’s how it’s done at the moment; I just think it shouldn’t be done, so I’m asking if there are any relevant regulations

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.