HCBBS Forum (English)
Submit Chemical Projects / Find Solutions
Amplify Your Requirements on a Broader Chemical Platform *Engineering · Technology · Equipment · Solutions*
Submit Request

Texaco gasifier wall thickness issue!

2011-05-28View Original

Thread Content

Why are the wall thicknesses of the cylinder and the vault different in a Texaco gasifier?
Reply #22011-06-01
Hahahahahahaha, another beginner! The dome is cast as a single unit, with three layers of bricks; the cylinder consists of four layers of bricks, built layer by layer. Due to the size of the reaction area, there is a reflux zone at the top, which is why it’s larger. . . . . . . . . . . . . . . . . . . . . . .
Reply #32011-06-06
Big brother! I’m talking about the thickness of the iron wall, not the thickness of the bricks!
Reply #42011-06-07
For pressure vessels, the thickness is calculated based on the stress conditions applied. The membrane stress acting on a spherical head is half of the circumferential stress in the connecting cylinder; therefore, the calculated thickness is also approximately half of that of the connecting cylinder.
Reply #52011-06-08
What is the wall thickness of 2.8-meter and 3.2-meter gasification furnaces?

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.