The rust is severe; even after 30 minutes of plating, no zinc is formed

2011-06-20View Original

Thread Content

The cold-drawn wire has been exposed to rain for over a month, so it is heavily rusted. It can be cleaned through pickling, but no zinc coating will form even after 30 minutes of plating; re-plating also doesn’t work. What should be done? Please, masters, help think of a solution
Reply #22011-06-21
First, grind to remove rust, then acid-wash the rust spots, and replating
Reply #32011-06-23
Oh, give it a try, but there’s so much of it – it will take a lot of manual work to polish it
Reply #42011-06-28
““First grind to remove rust, then pickle the rust spots, and replating” – this method doesn’t work; the result is the same whether grinding is done or not

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.