How to perform impact testing on Q345R and 09mnniDR? What welding materials are suitable?

2011-06-22View Original

Thread Content

For Q345R and 09mnniDR, how should impact testing be carried out? What welding materials are suitable – 507 or W707?
Reply #22011-06-22
W707 should be chosen, but due to the effect of base metal dilution on the Q345R side, the low-temperature impact toughness of the weld will decrease.
Reply #32011-06-22
Since Q345R is used, the impact temperature is maintained above -20 degrees Celsius. There is no need to use low-temperature welding materials. Options such as J507R\J507RH can be chosen.
Reply #42011-06-26
I think J507RH should work fine

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.