Tube sheet calculation and bolt material in SW6 software

2011-10-19View Original

Thread Content

Dear seniors: When using the SW6 calculation software to determine the thickness of heat exchanger tube sheets, if all other parameters remain unchanged but the material of the main bolts differs, why does the calculated thickness of the tube sheet vary?
Reply #22011-10-19
Under pre-tensioning, different bolt materials result in different calculated bolt loads; consequently, the flange torque varies, and the required thickness of the tube sheet also changes. The higher the strength of the bolts, the thicker the tube sheet should be, presumably.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.