For welding pure copper (T2), should HS212 or QSn6.5-0.1 be used?

2012-02-08View Original

Thread Content

For welding pure copper (T2), should HS212 or QSn6.5-0.1 be used?
Reply #22012-02-08
HS212 is used quite often; I’ve never seen QSn6.5-0.1 being used for welding. Perhaps my knowledge is limited; experts can come and add to it!

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.