I currently have a cylinder with a diameter of 600 mm and a length of 600 mm. The material used is a composite sheet of N06600+Q345R, with a thickness of 3+25 mm. Do those who have experience in manufacturing know whether it’s possible to roll such a cylinder? Could there be any problems with the composite sheet during the rolling process? Will heat treatment after the cylinder is manufactured have an adverse effect on the cladding? Thank you
Reply #22012-02-10
It is a nickel-based alloy composite plate that can be cold-formed; Given the relatively high deformation rate, medium-temperature forming (550°C–600°C) can also be employed. Stress-relief heat treatment is required after shaping, with no adverse effect on the material properties.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.